Nanoindenter G200 (MTS -Agilent)

Equipement for measurements of nanohardness and elastic modulus.

Nanoindenter G200 (MTS -Agilent)

Contacts and Location

Contact 1 Roberts Zabels
Enquire about this equipment
Organisational Unit Institute of Solid State Physics
    University of Latvia

Description

Equipement for measurements of nanohardness and elastic modulus.

Specification

  • Optimum indentation depth range 100-2000 nm;
  • Load resolution – 50 nN;
  • Displacement resolution - <0.01 nm;
  • Usable sample area –typically up to 32 mm.

Services

Micromechanical caracterization of thin films and coatings, nanomaterials and surface layers of bulk materials.