Polymer thermal properties investigation by differential scanning calorimetry.

Differential Scanning Calorimeter

Contacts and Location

Description

Polymer thermal properties investigation by differential scanning calorimetry.

Specification

main functions:

  • Determination of polymer structure main thermal parameters such as: glass transition, melting, crystalisation, oxidation and destructions temperatures, crystalinity degree

parameters:

  • Temperature diapasone -100-300 oC
  • Temperature precision +/-0.2 oC
  • Heating and cooling rate 0.2-50 oC/min
  • Cooling to -100 oC with out liquid nitrogen
  • Experiment atmosphere: air, N2 and O2

Services

Determination of polymer structure main thermal parameters such as: glass transition, melting, crystalisation, oxidation and destruction temperatures, crystalinity degree